by
Öner, Cezmi, author.
Format:
El Yazması
Alıntı:
, the amount of porosity increased with Sc added to the alloy, and an increase in dendrite arm lengths
by
Özgür, Melek.
Format:
El Yazması
Alıntı:
H30, C50H50, C30H70, and C20H80. The porous low density scaffolds had 93.5-96.3% porosity with a
by
Ergün, Yelda.
Format:
El Yazması
Alıntı:
monomer in the emulsion decreases the porosity, water permeability and increases the mechanical properties
by
Yıldırım, Oktay.
Format:
El Yazması
Alıntı:
pressing method. The porosity and density values of porous hydroxyapatite samples changed in range of 34-72
by
Çelik, Emrah.
Format:
El Yazması
Alıntı:
compacts having porosity level of 40% and/or lower was comparable with that of human cortical bone.Compared
by
Akkaş, Hatice Deniz.
Format:
El Yazması
Alıntı:
temperature for crack free samples with the least amount of porosity. Also, the composite system exhibited the
by
Sütçü, Mücahit.
Format:
El Yazması
Alıntı:
dimensions were produced based on the blends that give the highest density and hardness values. Porosity and
by
Şimşek, Deniz.
Format:
El Yazması
Alıntı:
presence of relatively high porosity. 10vol% MSS whisker addition yields comparable compressive strength